Past research has shown unusual activity of the (1 x 1)Pt(110) surface to break carbon-carbon and carbon-oxygen bonds. Methane formation from ethylene or ethane has been reported for supported platinum catalysts. A model for the methane formation on (1 x 1)Pt(110), was proposed by Yagasaki. In this study, the mechanism of methane formation has been further investigated, and Yagasaki's model tested, by studying the decomposition of ethylene and methanol on the stepped surfaces Pt(511) and Pt(331) with Temperature Programmed Desorption. The experiments have been carried out in a Ultra High Vacuum system, equipped with a mass spectrometer, LEED and AES. Hydrogen and carbon monoxide desorption show that on Pt(511) different adsorption sites are available than on Pt(331). Ethylene decomposition on Pt(511) leads to small amounts of methane formation compared to (1 x 1)Pt(110). The metastable (1 x 1) phase of Pt(511) is 2-3 times more active than the stable (hex) phase. When $\rm\sp{13}C\sb2H\sb4$ is used, $\rm\sp{13}CH\sb4$ is not detected. Methane formation is not seen on the Pt(331) surface. Arguments are given why Pt(511) is a superior model for supported catalysts compared to (1 x 1)Pt(110). The carbon-oxygen bond of methanol is not broken on either Pt(511) or Pt(331), whether the surface is clean or covered with oxygen. Hydrogen saturating the surface, prevents the chemisorption of ethylene and the formation of methane. Postadsorption of hydrogen does not lead to an increase in methane formation. Coadsorption of ethylene with carbon monoxide shows a maximum methane formation at 0.3 L carbon monoxide exposure. Poison experiments with 'oxide' and carbon indicate that the active site for methane formation is located at the step. The amount of carbon deposited during ethylene decomposition, increases in the order (1 x 1)Pt(511) $\to$ (hex)Pt(511) $\to$ Pt(331). This is also the order for decreasing methane activity. In a new model, it is proposed that in order to be active for methane formation, a surface has to prevent the polymerization of single carbon species to inactive graphite. The model predicts that surfaces with large enough (111) terraces have higher diffusion rates and allow the single carbon species to convert to graphite before the species can be hydrogenated.

Degree

thesis:*
Name thesis:degree_name
Ph.D.
Level thesis:degree_level
Dissertation
Discipline thesis:degree_discipline
Chemical Engineering
Grantor
University of Illinois at Urbana-Champaign
Year dc:date
2011

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Spaendonk, Vincent Van

Subjects

dc:subject × 3

Rights

dc:rights
Statement dc:rights
  • Copyright 1994 Spaendonk, Vincent Van
Language dc:language
eng

Identifiers

dc:identifier.*
Identifier
AAI9512557
(UMI)AAI9512557
OAI identifier oai:identifier
oai:www.ideals.illinois.edu:2142/21509

Chain of custody

source
Harvested from
University of Illinois - Urbana-Champaign
Base URL
www.ideals.illinois.edu/oai-pmh
Last updated
2026-07-22
Source record
OAI-PMH GetRecord
citation

Spaendonk, Vincent Van. Stepped single crystals as improved model for supported catalysts: Ethylene, methanol and assorted molecules on platinum(511) and platinum(331). Dissertation thesis, University of Illinois at Urbana-Champaign, 2011. http://hdl.handle.net/2142/21509