Back to results

Massachusetts Institute of Technology

Stress corrosion cracking and crack tip characterization of Alloy X-750 in light water reactor environments

Abstract

dc:description.abstract

Stress corrosion cracking (SCC) susceptibility of Inconel Alloy X-750 in the HTH condition has been evaluated in high purity water at 93 and 288°C under Boiling Water Reactor Normal Water Chemistry (NWC) and Hydrogen Water Chemistry (HWC) conditions. SCC crack growth rates of approximately 1.1 x 10-7 mm/s (K=28 MPa[square root symbol]m) under NWC conditions and 1.4xI 0-8 mm/s (K=28 MPa[square root symbol]m) under HWC in high purity water at 288°C were observed. The environmental conditions were changed from NWC to HWC during constant K loading, and the crack growth rate immediately slowed down by approximately one order of magnitude. The alloy was also tested in HWC at 93°C. No SCC crack growth was observed at K= 35 MPa[square root symbol]m for the length of time tested at 93°C. The fracture mode transitioned from predominantly transgranular cracking under fatigue conditions to a mixture of intergranular, pseudo-intergranular, and a small amount of transgranular fracture in constant stress intensity SCC. Pseudo-intergranular cracking is when a crack propagates directly adjacent to the grain boundary carbides and not actually on the grain boundary. The SCC crack tips were characterized with scanning electron microscopy (SEM) and 3D Atom Probe Tomography (APT). The SEM analysis was focused on the fractographic analysis and crack-propagation mode. The crack was observed to propagate adjacent to grain boundary carbides (pseudo-intergranular) and along a boundary with high coherency where no carbides were present (intergranular). The small and localized areas of transgranular cracking were occasionally seen between two regions of intergranular cracking. The APT reconstructions of the crack tips and crack wall identified several key features contributing to the SCC process: 1) Preferential oxygen transport occurs in either a finger-like or crystallographic morphology extending from the crack tip region. These regions are enriched in both oxygen and oxide with the oxide being a chromium-nickel spinel. 2) The matrix ahead of each finger-like "tunnel" is enriched in oxygen and predominantly chromium oxide. This indicates that oxygen is diffusing ahead of the crack tip into the bulk material. 3) The oxygen that penetrates directly into the base material from the crack walls in an ordered manner suggests that it is controlled by crystallographic features. 4) The main SCC crack tip is full of predominantly oxide phase and, to a lesser extent, metal atoms. The very crack tip forms a spinel of chromium and nickel oxides. Iron oxide begins to contribute to the oxide spinel approximately 25-30 nm from the actual tip. 5) The [gamma] precipitates that are directly adjacent to each crack tip and crack wall were deficient in aluminum content. The aluminum content in the bulk [gamma] was approximately 6.6 at% and the near-crack [gamma] aluminum content ranged from 2.5-3.5 at%. The range of affected [gamma] was approximately 100 nm wide.

Degree

thesis:*
Department dc:contributor.department
Massachusetts Institute of Technology. Dept. of Nuclear Science and Engineering.
Grantor dc:publisher
Massachusetts Institute of Technology
Year dc:date.issued
2011

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Gibbs, Jonathan Paul
Advisor dc:contributor.advisor
  • Ronald G. Ballinger and John H. Jackson.

Subjects

dc:subject × 1

Rights

dc:rights
Statement dc:rights
  • M.I.T. theses are protected by copyright. They may be viewed from this source for any purpose, but reproduction or distribution in any format is prohibited without written permission. See provided URL for inquiries about permission.
Language dc:language.iso
eng

Identifiers

dc:identifier.*
Handle dc:identifier.uri
http://hdl.handle.net/1721.1/76498
OAI identifier oai:identifier
oai:dspace.mit.edu:1721.1/76498

Chain of custody

source
Harvested from
MIT
Base URL
dspace.mit.edu/oai/request
Last updated
2026-07-22
Source record
OAI-PMH GetRecord
citation

Gibbs, Jonathan Paul. Stress corrosion cracking and crack tip characterization of Alloy X-750 in light water reactor environments. Massachusetts Institute of Technology, 2011. http://hdl.handle.net/1721.1/76498