{"id":{"repo_id":"vt","oai_identifier":"oai:vtechworks.lib.vt.edu:10919/35197"},"canonical_url":"https://search.dev.ndltd.org/etd/vt/oai:vtechworks.lib.vt.edu:10919/35197","repository":{"repo_id":"vt","name":"Virginia Tech","base_url":"https://vtechworks.lib.vt.edu/oai/request"},"display":{"title":"Evaluation of Novel and Low-Cost Materials for Bipolar Plates in PEM Fuel Cells","abstract":"Bipolar plate material and fabrication costs make up a significant fraction of the total cost in a polymer electrolyte membrane fuel cell stack. In an attempt to reduce these costs, a novel manufacturing method was developed for use with composite materials. Conductive fillers were mixed with a polypropylene binder and molded into single cell monopolar plates. A fuel cell test stand, capable of testing six cells simultaneously, was used for long-term corrosion testing. In-situ tests took place in 5 cm2 active area fuel cells with cathode humidification. Using data from test cells containing graphite monopolar plates as a baseline, two composite formulations, were able to produce power at 66-79% of the baseline power. Power output from one cell remained in this range for over 200 hours, while the other sample experienced surface oxidation and eventually failed. With improvements in part conductivity coming from conductive polymers, this manufacturing technique holds the promise of producing monopolar and bipolar plates that could eventually be scaled up for use in fuel cell stacks.","abstract_html":"Bipolar plate material and fabrication costs make up a significant fraction of the total cost in a polymer electrolyte membrane fuel cell stack. In an attempt to reduce these costs, a novel manufacturing method was developed for use with composite materials. Conductive fillers were mixed with a polypropylene binder and molded into single cell monopolar plates. A fuel cell test stand, capable of testing six cells simultaneously, was used for long-term corrosion testing. In-situ tests took place in 5 cm2 active area fuel cells with cathode humidification. Using data from test cells containing graphite monopolar plates as a baseline, two composite formulations, were able to produce power at 66-79% of the baseline power. Power output from one cell remained in this range for over 200 hours, while the other sample experienced surface oxidation and eventually failed. With improvements in part conductivity coming from conductive polymers, this manufacturing technique holds the promise of producing monopolar and bipolar plates that could eventually be scaled up for use in fuel cell stacks.","abstract_has_math":false,"creators":["Desrosiers, Kevin Campbell"],"institution":"Virginia Tech","degree_name":"Master of Science","degree_level":"masters","degree_discipline":"Mechanical Engineering","degree_department":"Mechanical Engineering","school":null,"contributors":[],"advisors":[],"committee_chairs":["Nelson, Douglas J."],"committee_members":["von Spakovsky, Michael R.","Ellis, Michael W."],"year":2002,"date_issued":"2002-09-16","date_published":"2002-09-16","updated_at":"2026-07-22T22:20:16Z","subjects":["PEMFC","Composite","Fuel Cell","Injection Molding","Graphite","Separator Plates","Test Stand"],"languages":[],"rights":["In Copyright"],"rights_urls":["http://rightsstatements.org/vocab/InC/1.0/"],"identifier_entries":[{"key":"dc:identifier.other","label":"Dc Identifier Other","values":["etd-09262002-105745"],"render_values":[{"text":"etd-09262002-105745","href":null,"code":true}]}]},"links":{"outbound_url":"http://hdl.handle.net/10919/35197","outbound_label":"Handle","outbound_source":"dc:identifier.uri"},"metadata_groups":[{"id":"people","label":"People","entries":[{"key":"dc:contributor.committeechair","label":"Committee Chair","values":["Nelson, Douglas J."]},{"key":"dc:contributor.committeemember","label":"Committee Member","values":["von Spakovsky, Michael R.","Ellis, Michael W."]},{"key":"dc:contributor.department","label":"Department","values":["Mechanical Engineering"]},{"key":"dc:creator","label":"Author","values":["Desrosiers, Kevin Campbell"]}]},{"id":"academic_context","label":"Academic Context","entries":[{"key":"dc:date.accessioned","label":"Dc Date Accessioned","values":["2014-03-14T20:46:00Z"]},{"key":"dc:date.available","label":"Dc Date Available","values":["2014-03-14T20:46:00Z","2005-09-30"]},{"key":"dc:date.issued","label":"Date","values":["2002-09-16"]},{"key":"dc:publisher","label":"Institution","values":["Virginia Tech"]},{"key":"dc:type","label":"Dc Type","values":["Thesis"]},{"key":"thesis:degree_discipline","label":"Discipline","values":["Mechanical Engineering"]},{"key":"thesis:degree_level","label":"Degree Level","values":["masters"]},{"key":"thesis:degree_name","label":"Degree Name","values":["Master of Science"]},{"key":"thesis:institution_name","label":"Thesis Institution Name","values":["Virginia Polytechnic Institute and State University"]}]},{"id":"subjects_keywords","label":"Subjects and Keywords","entries":[{"key":"dc:subject","label":"Dc Subject","values":["PEMFC","Composite","Fuel Cell","Injection Molding","Graphite","Separator Plates","Test Stand"]}]},{"id":"language_rights","label":"Language and Rights","entries":[{"key":"dc:rights","label":"Dc Rights","values":["In Copyright"]},{"key":"dc:rights.uri","label":"Rights URI","values":["http://rightsstatements.org/vocab/InC/1.0/"]}]},{"id":"identifiers","label":"Identifiers","entries":[{"key":"dc:identifier.other","label":"Dc Identifier Other","values":["etd-09262002-105745"]},{"key":"dc:identifier.uri","label":"Identifier URI","values":["http://hdl.handle.net/10919/35197"]}]},{"id":"additional","label":"Additional Metadata","entries":[{"key":"dc:description.abstract","label":"Abstract","values":["Bipolar plate material and fabrication costs make up a significant fraction of the total cost in a polymer electrolyte membrane fuel cell stack. In an attempt to reduce these costs, a novel manufacturing method was developed for use with composite materials. Conductive fillers were mixed with a polypropylene binder and molded into single cell monopolar plates. A fuel cell test stand, capable of testing six cells simultaneously, was used for long-term corrosion testing. In-situ tests took place in 5 cm2 active area fuel cells with cathode humidification. Using data from test cells containing graphite monopolar plates as a baseline, two composite formulations, were able to produce power at 66-79% of the baseline power. Power output from one cell remained in this range for over 200 hours, while the other sample experienced surface oxidation and eventually failed. With improvements in part conductivity coming from conductive polymers, this manufacturing technique holds the promise of producing monopolar and bipolar plates that could eventually be scaled up for use in fuel cell stacks."]},{"key":"dc:description.degree","label":"Dc Description Degree","values":["Master of Science"]},{"key":"dc:title","label":"Title","values":["Evaluation of Novel and Low-Cost Materials for Bipolar Plates in PEM Fuel Cells"]}]}],"canonical_facts":{"dc:contributor.committeechair":["Nelson, Douglas J."],"dc:contributor.committeemember":["von Spakovsky, Michael R.","Ellis, Michael W."],"dc:contributor.department":["Mechanical Engineering"],"dc:creator":["Desrosiers, Kevin Campbell"],"dc:date.accessioned":["2014-03-14T20:46:00Z"],"dc:date.available":["2014-03-14T20:46:00Z","2005-09-30"],"dc:date.issued":["2002-09-16"],"dc:description.abstract":["Bipolar plate material and fabrication costs make up a significant fraction of the total cost in a polymer electrolyte membrane fuel cell stack. In an attempt to reduce these costs, a novel manufacturing method was developed for use with composite materials. Conductive fillers were mixed with a polypropylene binder and molded into single cell monopolar plates. A fuel cell test stand, capable of testing six cells simultaneously, was used for long-term corrosion testing. In-situ tests took place in 5 cm2 active area fuel cells with cathode humidification. Using data from test cells containing graphite monopolar plates as a baseline, two composite formulations, were able to produce power at 66-79% of the baseline power. Power output from one cell remained in this range for over 200 hours, while the other sample experienced surface oxidation and eventually failed. With improvements in part conductivity coming from conductive polymers, this manufacturing technique holds the promise of producing monopolar and bipolar plates that could eventually be scaled up for use in fuel cell stacks."],"dc:description.degree":["Master of Science"],"dc:identifier.other":["etd-09262002-105745"],"dc:identifier.uri":["http://hdl.handle.net/10919/35197"],"dc:publisher":["Virginia Tech"],"dc:rights":["In Copyright"],"dc:rights.uri":["http://rightsstatements.org/vocab/InC/1.0/"],"dc:subject":["PEMFC","Composite","Fuel Cell","Injection Molding","Graphite","Separator Plates","Test Stand"],"dc:title":["Evaluation of Novel and Low-Cost Materials for Bipolar Plates in PEM Fuel Cells"],"dc:type":["Thesis"],"thesis:degree_discipline":["Mechanical Engineering"],"thesis:degree_level":["masters"],"thesis:degree_name":["Master of Science"],"thesis:institution_name":["Virginia Polytechnic Institute and State University"]},"updated_at":"2026-07-22T22:20:16Z"}