University of Nevada, Las Vegas
Cracking of zirconium alloys at constant load with and without applied potentials
Abstract
dc:description.abstractCladding materials, namely Zircaloy-2 (Zr-2) and Zircaloy-4 (Zr-4), were tested for evaluation of their resistance to stress corrosion cracking (SCC), delayed hydride cracking (DHC), and localized corrosion (pitting and crevice) in neutral and acidic environments at ambient temperature and 90°C. For SCC testing, constant load and slow-strain-rate techniques were used. Some SCC testing were also performed under controlled electrochemical potentials (Econt). The localized corrosion behavior was studied by cyclic potentiodynamic polarization technique. Metallurgical microstructures and fractography were analyzed by optical microscopy and scanning electron microscopy (SEM), respectively. The results obtained from this study indicate that no failures were observed under constant loading with smooth specimens. However, the notched specimens showed failures at reduced applied loads. The application of Econt to the smooth specimens showed some signs of hydrogen damage that might be the precursor to the development of DHC. Fractographic evaluations by SEM revealed dimpled microstructures indicating ductile failures.
Degree
thesis:*- Name thesis:degree_name
- Master of Science (MS)
- Level thesis:degree_level
- Thesis
- Discipline thesis:degree_discipline
- Mechanical Engineering
- Grantor dc:publisher
- University of Nevada, Las Vegas
- Year
- 2003
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- Aquino, Heidi T
- Contributors dc:contributor
-
- Ajit K. Roy
Rights
dc:rights- Statement dc:rights
-
- IN COPYRIGHT. For more information about this rights statement, please visit http://rightsstatements.org/vocab/InC/1.0/
- Language dc:language
- English
Identifiers
dc:identifier.*- Identifier
- https://oasis.library.unlv.edu/rtds/1576
- OAI identifier oai:identifier
- oai:oasis.library.unlv.edu:rtds-2575