{"id":{"repo_id":"uiuc","oai_identifier":"oai:www.ideals.illinois.edu:2142/71807"},"canonical_url":"https://search.dev.ndltd.org/etd/uiuc/oai:www.ideals.illinois.edu:2142/71807","repository":{"repo_id":"uiuc","name":"University of Illinois - Urbana-Champaign","base_url":"https://www.ideals.illinois.edu/oai-pmh"},"display":{"title":"Solution History Effects and Crystal Phase Transformation in Polybutene-1 and Domain Morphology in Polyurethanes","abstract":"Isotactic polybutene-1 (PB-1) can crystallize in four different crystal forms in which the molecules assume three different helical conformations. When PB-1 crystallizes from a dilute solution the crystal form which precipitates is determined by the thermal history imposed on the solution and the crystal structure of the initial PB-1 solid. It is proposed that on dissolution, the helix conformation originally present in the solid may be temporarily retained. With time, it transforms into the helix which is thermodynamically stable at the given solution temperature. On crystallization, such helices form the crystal nuclei and which generate the corresponding crystal form. Measurements of the solution's intrinsic viscosity show that the hydrodynamic volume of a PB-1 molecule in solution varies considerably with the solution's thermal history, lending support to the idea of retention of helices in solution. The tetragonal (---&gt;) twinned hexagonal crystal phase transformation significantly alters the physical and mechanical properties of melt-crystallized PB-1. A study of the transformation mechanism at the molecular level was made. Results from an Avrami analysis imply that nucleation of the twinned hexagonal phase crystals is instantaneous in time and growth of the twinned hexagonal phase constitutes the rate-determining step. Transmission electron microscopy (TEM) reveals multiple nucleation within each tetragonal fibril in the melt-crystallized sample or in each solution-grown tetragonal single crystal. Nucleation is thought to be initiated by stress exerted between irregularly stacked crystal lamellae. Although interlamellar taut tie molecules are believed to accelerate transformation, they are not essential for the process. Many linear polyurethanes composed of alternating hard and soft segments have been shown to be composed of two phases. The hard and soft segments tend to aggregate individually to form hard- and soft-segment domains which are believed to be responsible for the unusual physical and mechanical properties exhibited by polyurethanes. The morphology of such domains in two polyurethanes was characterized by direct TEM observation and other techniques. A correlation was found to exist between the extent of domain formation and the physical and mechanical properties.","abstract_html":"Isotactic polybutene-1 (PB-1) can crystallize in four different crystal forms in which the molecules assume three different helical conformations. When PB-1 crystallizes from a dilute solution the crystal form which precipitates is determined by the thermal history imposed on the solution and the crystal structure of the initial PB-1 solid. It is proposed that on dissolution, the helix conformation originally present in the solid may be temporarily retained. With time, it transforms into the helix which is thermodynamically stable at the given solution temperature. On crystallization, such helices form the crystal nuclei and which generate the corresponding crystal form. Measurements of the solution&#x27;s intrinsic viscosity show that the hydrodynamic volume of a PB-1 molecule in solution varies considerably with the solution&#x27;s thermal history, lending support to the idea of retention of helices in solution. The tetragonal (---&amp;gt;) twinned hexagonal crystal phase transformation significantly alters the physical and mechanical properties of melt-crystallized PB-1. A study of the transformation mechanism at the molecular level was made. Results from an Avrami analysis imply that nucleation of the twinned hexagonal phase crystals is instantaneous in time and growth of the twinned hexagonal phase constitutes the rate-determining step. Transmission electron microscopy (TEM) reveals multiple nucleation within each tetragonal fibril in the melt-crystallized sample or in each solution-grown tetragonal single crystal. Nucleation is thought to be initiated by stress exerted between irregularly stacked crystal lamellae. Although interlamellar taut tie molecules are believed to accelerate transformation, they are not essential for the process. Many linear polyurethanes composed of alternating hard and soft segments have been shown to be composed of two phases. The hard and soft segments tend to aggregate individually to form hard- and soft-segment domains which are believed to be responsible for the unusual physical and mechanical properties exhibited by polyurethanes. The morphology of such domains in two polyurethanes was characterized by direct TEM observation and other techniques. A correlation was found to exist between the extent of domain formation and the physical and mechanical properties.","abstract_has_math":false,"creators":["Chau, Kin Wah"],"institution":"University of Illinois at Urbana-Champaign","degree_name":"Ph.D.","degree_level":"Dissertation","degree_discipline":"Metallurgical Engineering","degree_department":null,"school":null,"contributors":[],"advisors":[],"committee_chairs":[],"committee_members":[],"year":2014,"date_issued":"2014-12-16T20:51:54Z","date_published":"2014-12-16T20:51:54Z","updated_at":"2026-07-22T22:26:05Z","subjects":["Engineering, Materials Science"],"languages":[],"rights":[],"rights_urls":[],"identifier_entries":[{"key":"dc:identifier","label":"Identifier","values":["(UMI)AAI8409890"],"render_values":[{"text":"(UMI)AAI8409890","href":null,"code":true}]}]},"links":{"outbound_url":"http://hdl.handle.net/2142/71807","outbound_label":"Handle","outbound_source":"dc:identifier"},"metadata_groups":[{"id":"people","label":"People","entries":[{"key":"dc:creator","label":"Author","values":["Chau, Kin Wah"]}]},{"id":"academic_context","label":"Academic Context","entries":[{"key":"dc:date","label":"Dc Date","values":["2014-12-16T20:51:54Z","10000-01-01","1983"]},{"key":"dc:type","label":"Dc Type","values":["text"]},{"key":"thesis:degree_discipline","label":"Discipline","values":["Metallurgical Engineering"]},{"key":"thesis:degree_level","label":"Degree Level","values":["Dissertation"]},{"key":"thesis:degree_name","label":"Degree Name","values":["Ph.D."]},{"key":"thesis:institution_name","label":"Thesis Institution Name","values":["University of Illinois at Urbana-Champaign"]}]},{"id":"subjects_keywords","label":"Subjects and Keywords","entries":[{"key":"dc:subject","label":"Dc Subject","values":["Engineering, Materials Science"]}]},{"id":"identifiers","label":"Identifiers","entries":[{"key":"dc:identifier","label":"Identifier","values":["http://hdl.handle.net/2142/71807","(UMI)AAI8409890"]}]},{"id":"additional","label":"Additional Metadata","entries":[{"key":"dc:description","label":"Description","values":["Isotactic polybutene-1 (PB-1) can crystallize in four different crystal forms in which the molecules assume three different helical conformations. When PB-1 crystallizes from a dilute solution the crystal form which precipitates is determined by the thermal history imposed on the solution and the crystal structure of the initial PB-1 solid. It is proposed that on dissolution, the helix conformation originally present in the solid may be temporarily retained. With time, it transforms into the helix which is thermodynamically stable at the given solution temperature. On crystallization, such helices form the crystal nuclei and which generate the corresponding crystal form. Measurements of the solution's intrinsic viscosity show that the hydrodynamic volume of a PB-1 molecule in solution varies considerably with the solution's thermal history, lending support to the idea of retention of helices in solution. The tetragonal (---&gt;) twinned hexagonal crystal phase transformation significantly alters the physical and mechanical properties of melt-crystallized PB-1. A study of the transformation mechanism at the molecular level was made. Results from an Avrami analysis imply that nucleation of the twinned hexagonal phase crystals is instantaneous in time and growth of the twinned hexagonal phase constitutes the rate-determining step. Transmission electron microscopy (TEM) reveals multiple nucleation within each tetragonal fibril in the melt-crystallized sample or in each solution-grown tetragonal single crystal. Nucleation is thought to be initiated by stress exerted between irregularly stacked crystal lamellae. Although interlamellar taut tie molecules are believed to accelerate transformation, they are not essential for the process. Many linear polyurethanes composed of alternating hard and soft segments have been shown to be composed of two phases. The hard and soft segments tend to aggregate individually to form hard- and soft-segment domains which are believed to be responsible for the unusual physical and mechanical properties exhibited by polyurethanes. The morphology of such domains in two polyurethanes was characterized by direct TEM observation and other techniques. A correlation was found to exist between the extent of domain formation and the physical and mechanical properties.","Made available in DSpace on 2014-12-16T20:51:54Z (GMT). No. of bitstreams: 1 8409890.pdf: 4853993 bytes, checksum: 60dc5ccdfb57c2e545802d6472d04395 (MD5) Previous issue date: 1983","Embargo set by: Seth Robbins for item 71973 Lift date: Forever Reason: Restricted to the U of I community idenfinitely during batch ingest of legacy ETDs","Restricted to the U of I community idenfinitely during batch ingest of legacy ETDs","U of I Only","158 p.","Thesis (Ph.D.)--University of Illinois at Urbana-Champaign, 1983."]},{"key":"dc:title","label":"Title","values":["Solution History Effects and Crystal Phase Transformation in Polybutene-1 and Domain Morphology in Polyurethanes"]}]}],"canonical_facts":{"dc:creator":["Chau, Kin Wah"],"dc:date":["2014-12-16T20:51:54Z","10000-01-01","1983"],"dc:description":["Isotactic polybutene-1 (PB-1) can crystallize in four different crystal forms in which the molecules assume three different helical conformations. When PB-1 crystallizes from a dilute solution the crystal form which precipitates is determined by the thermal history imposed on the solution and the crystal structure of the initial PB-1 solid. It is proposed that on dissolution, the helix conformation originally present in the solid may be temporarily retained. With time, it transforms into the helix which is thermodynamically stable at the given solution temperature. On crystallization, such helices form the crystal nuclei and which generate the corresponding crystal form. Measurements of the solution's intrinsic viscosity show that the hydrodynamic volume of a PB-1 molecule in solution varies considerably with the solution's thermal history, lending support to the idea of retention of helices in solution. The tetragonal (---&gt;) twinned hexagonal crystal phase transformation significantly alters the physical and mechanical properties of melt-crystallized PB-1. A study of the transformation mechanism at the molecular level was made. Results from an Avrami analysis imply that nucleation of the twinned hexagonal phase crystals is instantaneous in time and growth of the twinned hexagonal phase constitutes the rate-determining step. Transmission electron microscopy (TEM) reveals multiple nucleation within each tetragonal fibril in the melt-crystallized sample or in each solution-grown tetragonal single crystal. Nucleation is thought to be initiated by stress exerted between irregularly stacked crystal lamellae. Although interlamellar taut tie molecules are believed to accelerate transformation, they are not essential for the process. Many linear polyurethanes composed of alternating hard and soft segments have been shown to be composed of two phases. The hard and soft segments tend to aggregate individually to form hard- and soft-segment domains which are believed to be responsible for the unusual physical and mechanical properties exhibited by polyurethanes. The morphology of such domains in two polyurethanes was characterized by direct TEM observation and other techniques. A correlation was found to exist between the extent of domain formation and the physical and mechanical properties.","Made available in DSpace on 2014-12-16T20:51:54Z (GMT). No. of bitstreams: 1 8409890.pdf: 4853993 bytes, checksum: 60dc5ccdfb57c2e545802d6472d04395 (MD5) Previous issue date: 1983","Embargo set by: Seth Robbins for item 71973 Lift date: Forever Reason: Restricted to the U of I community idenfinitely during batch ingest of legacy ETDs","Restricted to the U of I community idenfinitely during batch ingest of legacy ETDs","U of I Only","158 p.","Thesis (Ph.D.)--University of Illinois at Urbana-Champaign, 1983."],"dc:identifier":["http://hdl.handle.net/2142/71807","(UMI)AAI8409890"],"dc:subject":["Engineering, Materials Science"],"dc:title":["Solution History Effects and Crystal Phase Transformation in Polybutene-1 and Domain Morphology in Polyurethanes"],"dc:type":["text"],"thesis:degree_discipline":["Metallurgical Engineering"],"thesis:degree_level":["Dissertation"],"thesis:degree_name":["Ph.D."],"thesis:institution_name":["University of Illinois at Urbana-Champaign"]},"updated_at":"2026-07-22T22:26:05Z"}