Massachusetts Institute of Technology

Weld development for Incoloy alloy 908, a low thermal expansion superalloy

Abstract

dc:description

Thesis (Ph. D.)--Massachusetts Institute of Technology, Dept. of Nuclear Engineering, 1995.

Degree

thesis:*
Department dc:contributor.department
Massachusetts Institute of Technology. Department of Nuclear Engineering
Grantor dc:publisher
Massachusetts Institute of Technology
Year dc:date.issued
1995

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Jang, Chang Heui
Advisor dc:contributor.advisor
  • Ronald G. Ballinger.

Subjects

dc:subject × 1

Rights

dc:rights
Statement dc:rights
  • M.I.T. theses are protected by copyright. They may be viewed from this source for any purpose, but reproduction or distribution in any format is prohibited without written permission. See provided URL for inquiries about permission.
Language dc:language.iso
en_US

Identifiers

dc:identifier.*
Handle dc:identifier.uri
http://hdl.handle.net/1721.1/28140

Chain of custody

source
Harvested from
MIT
Base URL
dspace.mit.edu/oai/request
Last updated
2026-07-22
Source record
OAI-PMH GetRecord
related terms
citation

Jang, Chang Heui. Weld development for Incoloy alloy 908, a low thermal expansion superalloy. Massachusetts Institute of Technology, 1995. http://hdl.handle.net/1721.1/28140