{"id":{"repo_id":"etsu","oai_identifier":"oai:dc.etsu.edu:etd-2576"},"canonical_url":"https://search.dev.ndltd.org/etd/etsu/oai:dc.etsu.edu:etd-2576","repository":{"repo_id":"etsu","name":"East Tennessee State University","base_url":"https://dc.etsu.edu/do/oai/"},"display":{"title":"Fabrication of Chemically Modified Nanometer-sized Gold Electrodes and Their Application in Electrocatalysis at Pt Nanoparticles.","abstract":"<p>Hydrogen evolution via proton reduction occurs at a high rate at the surface of Pt than at Au electrodes. Using cyclic voltammetry, chemically modified nanometer-sized Au electrodes, prepared by the Laser-Assisted Puller Method, were employed to examine current amplification by electrocalysis at Pt nanoparticles adsorbed on the modified Au electrode surfaces. The electrodes were modified with Self-Assembled Monolayers (SAMs) of cysteamine and soaked in Pt colloid solutions overnight. Monitoring the decrements of the characteristic steady-state catalytic current for proton reduction indicated that aggregates of Pt nanoparticles are adsorbed on the cysteamine monolayers and desorb from them particle by particle. The results also indicate that some particles are strongly attached to the modified electrode surface and do not deplete even after thorough rinsing.</p>","abstract_html":"&lt;p&gt;Hydrogen evolution via proton reduction occurs at a high rate at the surface of Pt than at Au electrodes. Using cyclic voltammetry, chemically modified nanometer-sized Au electrodes, prepared by the Laser-Assisted Puller Method, were employed to examine current amplification by electrocalysis at Pt nanoparticles adsorbed on the modified Au electrode surfaces. The electrodes were modified with Self-Assembled Monolayers (SAMs) of cysteamine and soaked in Pt colloid solutions overnight. Monitoring the decrements of the characteristic steady-state catalytic current for proton reduction indicated that aggregates of Pt nanoparticles are adsorbed on the cysteamine monolayers and desorb from them particle by particle. The results also indicate that some particles are strongly attached to the modified electrode surface and do not deplete even after thorough rinsing.&lt;/p&gt;","abstract_has_math":false,"creators":["Lakbub, Jude"],"institution":null,"degree_name":"MS (Master of Science)","degree_level":"Thesis - unrestricted","degree_discipline":"Chemistry","degree_department":null,"school":null,"contributors":[],"advisors":[],"committee_chairs":[],"committee_members":[],"year":2011,"date_issued":"2011-12-17T08:00:00Z","date_published":"2011-12-17T08:00:00Z","updated_at":"2026-07-24T02:20:31Z","subjects":["Chemically modified electrode","Nanometer-sized electrode","Self-Assembled Monolayer","Platinum Nanoparticles","Chemistry","Physical Sciences and Mathematics"],"languages":[],"rights":["Copyright by the authors."],"rights_urls":[],"identifier_entries":[]},"links":{"outbound_url":"https://dc.etsu.edu/etd/1385","outbound_label":"Repository record","outbound_source":"dc:identifier"},"metadata_groups":[{"id":"people","label":"People","entries":[{"key":"dc:creator","label":"Author","values":["Lakbub, Jude"]}]},{"id":"academic_context","label":"Academic Context","entries":[{"key":"dc:date.available","label":"Dc Date Available","values":["1990-01-01T08:00:00Z"]},{"key":"dc:date.issued","label":"Date","values":["2011-12-17T08:00:00Z"]},{"key":"thesis:degree_discipline","label":"Discipline","values":["Chemistry"]},{"key":"thesis:degree_level","label":"Degree Level","values":["Thesis - unrestricted"]},{"key":"thesis:degree_name","label":"Degree Name","values":["MS (Master of Science)"]}]},{"id":"subjects_keywords","label":"Subjects and Keywords","entries":[{"key":"dc:subject","label":"Dc Subject","values":["Chemically modified electrode","Nanometer-sized electrode","Self-Assembled Monolayer","Platinum Nanoparticles","Chemistry","Physical Sciences and Mathematics"]}]},{"id":"language_rights","label":"Language and Rights","entries":[{"key":"dc:rights","label":"Dc Rights","values":["Copyright by the authors."]}]},{"id":"identifiers","label":"Identifiers","entries":[{"key":"dc:identifier","label":"Identifier","values":["https://dc.etsu.edu/context/etd/article/2576/viewcontent/LakbubJ120611f.pdf","https://dc.etsu.edu/etd/1385"]}]},{"id":"additional","label":"Additional Metadata","entries":[{"key":"dc:description.abstract","label":"Abstract","values":["<p>Hydrogen evolution via proton reduction occurs at a high rate at the surface of Pt than at Au electrodes. Using cyclic voltammetry, chemically modified nanometer-sized Au electrodes, prepared by the Laser-Assisted Puller Method, were employed to examine current amplification by electrocalysis at Pt nanoparticles adsorbed on the modified Au electrode surfaces. The electrodes were modified with Self-Assembled Monolayers (SAMs) of cysteamine and soaked in Pt colloid solutions overnight. Monitoring the decrements of the characteristic steady-state catalytic current for proton reduction indicated that aggregates of Pt nanoparticles are adsorbed on the cysteamine monolayers and desorb from them particle by particle. The results also indicate that some particles are strongly attached to the modified electrode surface and do not deplete even after thorough rinsing.</p>"]},{"key":"dc:title","label":"Title","values":["Fabrication of Chemically Modified Nanometer-sized Gold Electrodes and Their Application in Electrocatalysis at Pt Nanoparticles."]}]}],"canonical_facts":{"dc:creator":["Lakbub, Jude"],"dc:date.available":["1990-01-01T08:00:00Z"],"dc:date.issued":["2011-12-17T08:00:00Z"],"dc:description.abstract":["<p>Hydrogen evolution via proton reduction occurs at a high rate at the surface of Pt than at Au electrodes. Using cyclic voltammetry, chemically modified nanometer-sized Au electrodes, prepared by the Laser-Assisted Puller Method, were employed to examine current amplification by electrocalysis at Pt nanoparticles adsorbed on the modified Au electrode surfaces. The electrodes were modified with Self-Assembled Monolayers (SAMs) of cysteamine and soaked in Pt colloid solutions overnight. Monitoring the decrements of the characteristic steady-state catalytic current for proton reduction indicated that aggregates of Pt nanoparticles are adsorbed on the cysteamine monolayers and desorb from them particle by particle. The results also indicate that some particles are strongly attached to the modified electrode surface and do not deplete even after thorough rinsing.</p>"],"dc:identifier":["https://dc.etsu.edu/context/etd/article/2576/viewcontent/LakbubJ120611f.pdf","https://dc.etsu.edu/etd/1385"],"dc:rights":["Copyright by the authors."],"dc:subject":["Chemically modified electrode","Nanometer-sized electrode","Self-Assembled Monolayer","Platinum Nanoparticles","Chemistry","Physical Sciences and Mathematics"],"dc:title":["Fabrication of Chemically Modified Nanometer-sized Gold Electrodes and Their Application in Electrocatalysis at Pt Nanoparticles."],"thesis:degree_discipline":["Chemistry"],"thesis:degree_level":["Thesis - unrestricted"],"thesis:degree_name":["MS (Master of Science)"]},"updated_at":"2026-07-24T02:20:31Z"}