  1. The effect of cooling rate on toughness and crystallinity in poly(ether ketone ketone) (PEKK)/G30-500 composites

    … the composite after completion of the standard fabrication process. The sixth panel was used to investigate changes in toughness due to manufacturing towpreg with polymer that had been reclaimed from the towpreg fabrication system’s air cleaner. Cooling rates of 2°C/min, 4°C/min, 6°C/min, …