Effects of stress state on fracture behavior of high carbon steel
Includes bibliographical references (pages 128-131).
-
Effects of stress state on fracture behavior of high carbon steel
Includes bibliographical references (pages 128-131).
-
Enhancing Corrosion Resistance and Hardness Properties of High-Carbon Steel and Aluminium Bronze Alloy Through Novel Surface Modification Technique
High carbon steel has been extensively utilised in various industrial applications, due to its consequential importance to strength-hardness balance and relatively low cost. With a mediocre level of corrosion resistance, the improvement is very important to extend its serviceability. Studied steels …
-
Single shear vs. double shear for nails in lateral loading
… at or near proportional limit show that low-carbon-steel plain-shank and helically threaded Screwtite nails loaded in double shear carry twice the single-shear loads; while hardened high-carbon-steel plain-shank and Screwtite nails loaded in double shear carry considerably less than twice the …
-
Characterization of Carbonaceous Exsolvate from Metal Melts
This study seeks to explore the role of carbon meso-structures in the strengthening of steel by characterizing the carbonaceous exsolvate from a metal-carbon melt. Metal-carbon matrix composites, such as the material used in this investigation, are commonly employed to strengthen tool steel. …
-
Induction Infrared Thermography for Non-Destructive Evaluation of Alloy Sensitization
The sensitization of stainless steel describes the process by which a high-carbon steel alloy is heated above a certain threshold (either naturally or artificially) followed by a cooling period during which chromium (one of the elements most responsible for providing stainless steel with its …
-
Sustainable design and durability of domestic micro combined heat and power scroll expander systems.
… were identified on the tip seal and the steel plate of the scroll expander. Abrasive wear derived from a two-body contact on the interface of the tip seal and the steel plate. Three-body wear was found across the steel plate of the scroll. Finally, cavitation pits were revealed. …
-
The effect of drawing strain on the fatigue behaviour of stainless and carbon steel wires
… crack growth behaviour of three different steels in wire form, namely, an austenitic AISI 304 stainless steel, a corrosion resistant ferritic steel, 3CR12, and pearlitic high carbon steel. The stainless steel wires were produced in the laboratory at a drawing speed of 50 mm min-1, without …
-
Understanding the Stability of Retained Austenite in High-Carbon Steels: Modelling and Alloy Design
In high-carbon steels, the austenite-to-martensite transformation under applied stress initiates at a critical value, contrary to low-carbon steels where the transformation occurs at the early stages of deformation. There are few models that account for the delayed transformation, because previous …