Global ETD Search

Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.

Results

Showing 1 to 7 of 7 for “"deoxidation"”.

  1. Deoxidation mechanisms in liquid steel.

    … techniques have been employed to investigate the deoxidation kinetics and changes in oxidation product morphology in low carbon steel melts. The techniques have been used to study the deoxidation processes associated with aluminium, titanium, silicon, zirconium and a calcium-aluminium alloy.After …

    sheffield-hallam Repository record for Deoxidation mechanisms in liquid steel. (opens in a new tab)

  2. Phase relationships during deoxidation and solidification of iron alloys.

    Massachusetts Institute of Technology. Dept. of Metallurgy and Materials Science. Thesis. 1973. Sc.D.

    mit Repository record for Phase relationships during deoxidation and solidification of iron alloys. (opens in a new tab)

  3. Galvanic deoxidation of molten steel using a solid electrolyte cell

    Thesis (M.S.)--Massachusetts Institute of Technology, Dept. of Materials Science and Engineering, 1994.

    mit Repository record for Galvanic deoxidation of molten steel using a solid electrolyte cell (opens in a new tab)

  4. Deoxidation studies : The interaction of vitreous silica with molten aluminium and systems of aluminium, manganese, iron and silicon.

    The interaction of aluminium with silica and silicates isthermodynamically inevitable and leads to reaction effects in many systems. The resultant reactions can continue over a wide temperature range including both liquid and solid state systems such as molten aluminium handling units and the heat …

    sheffield-hallam Repository record for Deoxidation studies : The interaction of vitreous silica with molten aluminium and systems of aluminium, manganese, iron and silicon. (opens in a new tab)

  5. Oxide inclusion evolution and factors that influence their size and morphology

    … composition, and morphology following steel deoxidation were found to depend on the steel conditions during deoxidation, and the method/sequence of deoxidant addition. The oxide size distribution evolved from lognormal to fractal and the distribution shape was quadratic or linear on a log-log …

    must-thes Repository record for Oxide inclusion evolution and factors that influence their size and morphology (opens in a new tab)

  6. Development of Stage-I tempered high strength cast steel for ground engaging tools

    … practice (N< 80 ppm) along with an effective deoxidation. Size of ground Si-Zr addition controls final ZrN particle size. Good mechanical properties can be obtained if ZrN particle size is limited to 2μm. A high oxygen melt practice gave 35% improvement in notch toughness. A Mn-Si-Mo-V steel …

    must-thes Repository record for Development of Stage-I tempered high strength cast steel for ground engaging tools (opens in a new tab)

  7. Optimalizace výroby těžkých ocelových odlitků

    Diplomová práce byla řešena v rámci projektu FR-TI1/070 „Optimalizace výroby těžkých odlitků“ ve spolupráci se slévárnou ŽĎAS a.s. Práce je zaměřena na hodnocení výskytu lasturového lomu ve vzorcích odebraných ze zkušebních odlitků. Zkušební tyče pro statickou zkoušku tahem byly odebrány z tepelné …

    brno-tech Repository record for Optimalizace výroby těžkých ocelových odlitků (opens in a new tab)