Global ETD Search

Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.

Results

Showing 1 to 1 of 1 for “"Refractory superalloys"”.

  1. Microstructural Evolution in Refractory Metal Multi-Component Alloy Systems

    … than those tolerated by current Ni-based superalloys, motivating the search for alternative high temperature materials. Refractory superalloys based on AlTaTiZr and AlMoNbTaTiZr have attracted particular interest, as early studies indicate that the essential attributes for elevated …

    cambridge Repository record for Microstructural Evolution in Refractory Metal Multi-Component Alloy Systems (opens in a new tab)