Enhancing hot tooling to forge high-γ ′ superalloys
High-γ ′ nickel superalloys are increasingly employed in aircraft turbines for their remarkable high-temperature properties to enhance engine efficiency and reduce aviation emissions. These alloys are forged at temperatures approaching 1100 °C and require careful selection of process parameters to …