Global ETD Search
Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.
Results
Showing 1 to 4 of 4 for “"AA2024-T3"”.
-
Effect of Galvanic Corrosion on Crack Propagation of Cold Expanded Holes in AA2024-T3
… crack initiation will be established for AA2024-T3 cold worked holes subjected to cyclic loads to determine the impact on fatigue life of joints in presence of saline solution, including Stress Intensity Factor (SIF) adjustments in the Linear Elastic Fracture Mechanic (LEFM) equations to …
-
Blister Test for Measurements of Adhesion and Adhesion Degradation of Organic Polymers on AA2024-T3
… by the BT and Optical Profilometry, using AA2024-T3 substrates coated with polyvinyl butyral (PVB). Random abrasion generated a surface with lower average roughness than aligned abrasion due to the continual cross abrasion of the grooves. The BT could discern the effects of different …
-
Effect of Turbulence on the Passive Film Growth and Associated Durability of Aluminum Alloys in Simulated Seawater
… experimental section of 45.7 mm inner diameter AA2024-T3 tubing in simulated seawater. Extensive degradation was observed in-situ and confirmed with ex-situ techniques after sequential exposure to fully-developed turbulent flow at an expected wall shear stress of 10 Pa for 180ks (Reynolds number …
-
Feedback active coatings based on mesoporous silica containers
… für die industriell wichtige Aluminiumlegierung AA2024-T3 dargestellt Mesoporöse Silika-Behälter wurden mit dem ungiftigen Inhibitor (2-Mercaptobenzothiazol) beladen und dann in die Matrix anorganischer (SiOx/ZrOx) oder organischer (wasserbasiert) Schichten dispergiert. Zwei Sorten von …