Global ETD Search

Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.

Results

Showing 1 to 4 of 4 for “"2.25 cr-1 mo"”.

  1. Elevated Temperature Fatigue Behavior of 2.25 Cr-1 Mo Steel

    Made available in DSpace on 2017-07-06T18:55:57Z (GMT). No. of bitstreams: 3 Raghuraman_S_MS.pdf: 60123616 bytes, checksum: f3e470db0d8155da904f0e846f2f975e (MD5) Raghuraman_S_MS_ABS.pdf: 963456 bytes, checksum: 2641591282a1687b0042df3c2a0fd1ba (MD5) license.txt: 4813 bytes, checksum: …

    uiuc Repository record for Elevated Temperature Fatigue Behavior of 2.25 Cr-1 Mo Steel (opens in a new tab)

  2. Evaluation of Temper Embrittlement in 2.25 Cr- 1 Mo Weld Metals Utilizing X-Ray Diffraction.

    … are a reduction in notch toughness, an increase in the ductile-to-brittle transition temperature as measured by Charpy vee-notch impact tests, and a change in fracture mode from ductile transgranular to brittle intergranular.

    uab Repository record for Evaluation of Temper Embrittlement in 2.25 Cr- 1 Mo Weld Metals Utilizing X-Ray Diffraction. (opens in a new tab)

  3. The Effects of Strain Induced Softening on the Load Carrying Capability of Components

    … has grown in using quenched and tempered 2.25 Cr 1 Mo steel in pressure vessels and piping systems. This material has a bainitic microstructure with improved short term strength characteristics over the more commonly used annealed form. The bainitic material cyclically softens, however, …

    uiuc Repository record for The Effects of Strain Induced Softening on the Load Carrying Capability of Components (opens in a new tab)

  4. Creep crack initiation and growth in 2.25% chromium - 1% molybdenum alloy steel

    <p>2.25%Cr-1 %Mo Steel has been utilised extensively for the manufacture of power plant components.</p> <p>This study has highlighted the implication of the presence of pre-existing defects in such components and, in particular, the influence of the microstructure on the creep deformation response …

    sheffield-hallam Repository record for Creep crack initiation and growth in 2.25% chromium - 1% molybdenum alloy steel (opens in a new tab)